5 Plastering defects & Measures To Pacify them

Be mindful of keeping the plaster moist to avoid cracks at the first place. Use fillers to fill the cracks and smoothen the surface after drying

Solution

Cracked
Plaster

#1

It indicates the presence of soluble salts in plaster. It can be pacified by brushing and washing the surface

Solution

Efflorescence
Plaster

#2

It appears due to improper mixing of plaster leaving behind dry lime particles. Ensure proper mixing and even proportion of plaster components.

Solution

Blistering of 
Plaster

#3

Ensure good workmanship and proper wall preparation and material selection before plastering

Solution

Falling off or Peeling of Plaster

#4

It occurs due to an uneven proportion of plaster components that leads to a lack of uniformity. Ensure the cement and water ratio remains same throughout the mix

Solution

Discolouration

#5